G'Day fellas
Whats the best or most suitable coating to put on a rod to protect the binding?
Cheers
G'Day fellas
Whats the best or most suitable coating to put on a rod to protect the binding?
Cheers
THE POOR MAN ALWAYS PAYS TWICE
If it's a new binding a couple of coats of thread filler,then a couple of coats of a two pack epoxy (Jack Erskine),you will need to be able to slowly rotate the rod for 24 hours if useing the Erskine product,for repairs or a quick finish you can get a prety good finish with 5 minute Z-epoxy.
P.S. you will still need to rotate with the Z epoxy.
nuffin' improves a nice wrap of insulation tape.........
In the good old days, (o.k., I'm old), we used to use estapol over speed king filler. Worked pretty well, but yellowed white horribly and didn't have that funky smoooooth finish unless in the hands of an expert i.e. not me. On the 5 minute araldite front, a heat gun will help it flow a bit.
If you are talking emergency repairs, then c thread and nailpolish will do, as I have proved after a rod and rod tube did not survive an encounter with the baggage handlers.
If you want a nice job with epoxy, then you are going to need to rotate it until it sets, in a nice warm spot away from dust.
Or you could speak to the local tackle store to see if their rod builder will do the job for you after you do the binding. Just try to speak to the rod builder before you hand over your bound up pride and joy. Well, probably before then. Otherwise, for example, your lovely bright gold/yellow thread might come back dull and boring.
Rick k
Thanks guys
Its an old rod that my misses was practicing a bit if tartan pattern binding on. Think I'll go with the 5 min Z epoxy.
Cheers
Mick
THE POOR MAN ALWAYS PAYS TWICE
There is a newish Araldite epoxy called "Crystal Clear" or somthing like that. Just a thought.
Alimo 88
Mick what's your location.
Myles
Myles
I'm in Gladstone Qld. Why do you ask?
THE POOR MAN ALWAYS PAYS TWICE
Mick, thought if you where northern suburbs Brisbane I could have helped you out that's all. Keep away from the araldite it will crack.
Myles
bearclaw, I know Araldite is not the correct epoxy to use but I did a road a few years back and it's still going strong.
Have you had any bad experiences with it ??????
Peter
Hi Pete,
I've used araldite also. It looked ok......for a while.
Maybe you got the mix exactly right to go the distance.
Worth a try if you don't want to go out and get one of the purpose made rod finishes.
IMO if you really like the binding and want it high lighted, use one of the rod epoxys.
Sorry for butting in on your answer Pete.
cheers r.
GO THE CRUISER UTES!
....OH WHAT A FEELING!
Peter,
I have had to repair several bad experiences that have occured when a rods owner has used the stuff, but your right it will get you out of a bind (pardon the pun) but Araldite is a 2 part epoxy glue and is quiet brittle, where epoxy finish is a 2 part epoxy casting resin in most cases.
It also yellows at an alarming rate making it no good for coating any form of thread art, will crack if flexed and if you ever want to rebuild the rod you will have a bugger of a time removing the Araldite from the blank.
Myles
Thanks Roz, I didn't think you were butting in, it's good to hear about all peoples experiences. So thanks for the reply
Thanks also to your reply Myles, I will take this on board.
I had just replaced some runners on a light action butterworth bream / whiting rod. Well to be honest it was a lovely 1 piece 10 foot 6 rod and lets just say it broke almost in half. That's another story in it's self but it involves me using heavy line and trying to free it from an under water immovable object. So I put a ferrel on and turned it into my new favorite 2 piece rod, after adding an extra runner to what it had and re spacing the others. All I need to do now is coat the bindings, so I will do it correctly under the expert advice from the above mentioned.
Thanks Again Peter
any tackle store will have some finishing material, it just depends on how good a job you did and how you want it to look later, way back in the "good old days" we always some two part stuff called "secret formula" I think it was imported by a company called I think Basser Millyard" or close to that, it was fantastic, but I know there is dozens of products out to do it.
By far the best stuff is Jack Erskines epoxy. If you want a long lasting finish nothing beats it. Dont use anything else.
What you shoul do is have a talk to Stuart as he is on the ball as far as rod finish .... you could say he has given them all ago ...
White Knight